In the plaster from the Gupta buildings of BHITARI a high percentage (74) of silica along with 14% of lime is present. Iron oxide and alumina contents measure up to 9%. Magnesia and alkalies are also present, while gypsum is completely absent.

- [Previous: v1.c19.s6.12](https://indike.org/pramana/ins.reference.ghosh-1989.v1.c19.s6.12)
- [Next: v1.c19.s6.14](https://indike.org/pramana/ins.reference.ghosh-1989.v1.c19.s6.14)
- [Up: v1.c19.s6](https://indike.org/pramana/ins.reference.ghosh-1989.v1.c19.s6)

## Linked texts (1)

- [Bhitari](https://indike.org/pramana/inp.site.bhitari)

---
Source: [https://indike.org/pramana/ins.reference.ghosh-1989.v1.c19.s6.13](https://indike.org/pramana/ins.reference.ghosh-1989.v1.c19.s6.13) · Pramāṇa