Pramāṇa · Search · About · API

Minerals and Metals in Ancient India v1.c27.s1.t4.3

Minerals and Metals in Ancient India v1.c27.s1.t4.3

Language
English

v1.c27.s1.t4.3

High-carbon wootz (crucible steel) cakes were probably forged at a not-too-high temperature in the range of 650-850°C (between ‘blood-red’ 650°C to ‘cherry-red’ 850°C) and then heat-treated by quenching. The European smiths failed to reproduce the result, probably because they were familiar with only low-carbon steel having a higher m.p., and tried to forge wootz at a white heat, when the cementite phase dissolved in the austenite, and the brittle structure ‘crumbled under the hammer’.